The photo shows serious warping (or curling) of my print from my old PEI sheet which was printed on my MK4 with my old heatbed. All four of the corners warped (only the worst corner is shown).

This has been a persistent problem for the last couple of years. Smaller models printed closer to the center of the bed are fine. Only bigger prints which approach the edges of the bed curl up.

I recently upgraded my MK4 to the MK4S. While I was at it, I replaced the heatbed and I bought a new PEI sheet. And even though the sheet was brand new, I did wash it thoroughly with warm water and Dawn dish soap before using it.

After running through the full calibration and reslicing my model for the new high-flow nozzle using the latest stable release of PrusaSlicer, I reprinted it with high expectations.

Unfortunately, I was disappointed. One of the corners warped. It wasn’t quite as severe as before, so that’s a slight improvement. The corner that did warp happens to be the same one shown in the pic.

Print Settings: Prusa MK4S printer (no enclosure) 0.4 mm high-flow nozzle 0.2 mm resolution 15% infill Prusament Army Green PLA

– Edit –

Wow, there are lots of good ideas here. Thanks everyone!

The things I’m going to try (in no paticular order).

  • Covering the printer with a cardboard box or insulation sheets to see if an enclosure would help.
  • Cutting a tiny relief across the sides on the first layer.
  • Adding a brim.
  • Slow down the first layer.
  • Spraying 3DLac on the corners

– Final Report –

I tried all of the above suggestions. Spraying 3DLac works! I will definitely keep this stuff in stock. Thanks again everyone!

  • Fuzzypyro@lemmy.world
    link
    fedilink
    English
    arrow-up
    6
    ·
    edit-2
    2 months ago

    3 things.

    1. Wash your build plate with soap and hot water. It helps more with adhesion than you think. Do not use glue stick or any adhesives on the plate. People report that it works but I always found significantly better results with just soap and hot water on pei with materials that adhere to pei well such as pla. Masking tape with adhesives might make a difference for materials that do not stick to pei.
    2. If you are designing the part or have any time with cad then put a tiny bevel chamfer on the surface that touches the build plate. Doesn’t meet to be large. Just something. It helps with cooling shrinkage and retraction of pla on the first layers.
    3. enclosure or still air will help but are not strictly needed for pla.

    Last thing I would do is maybe adjust your z-offset. It looks like it might be experiencing some elephants foot at the bottom. I would try raising the head just by about .10. Really though that is going to be fully determined by your first layer of course.

      • Fuzzypyro@lemmy.world
        link
        fedilink
        English
        arrow-up
        2
        ·
        2 months ago

        Hey OP, just so you do not waste time. I mis-spoke and told you the opposite of what you should do in the program. No bevel, I meant chamfer!

        I know it doesn’t make a lot of sense to make the surface area touching the build plate smaller but it is worth it since it provides relief from the layers above pulling when it is shrinking.